New AWS D1.1:2025 Changes That Affect Stud Welding on Bridge Projects

5 min readApril 2025

The 2025 edition of AWS D1.1 Structural Welding Code — Steel includes several updates that directly affect stud welding practice on bridge and highway projects. Here's a summary of the key changes.

Updated Visual Inspection Acceptance Criteria

The 2025 edition clarifies the acceptable flash ring geometry for headed shear studs. The previous language was ambiguous about partial flash rings on through-deck applications. The new criteria distinguish clearly between bare steel and through-deck welds, reducing unnecessary rejections on composite deck jobs.

Through-Deck Application Guidance

New annex material provides expanded guidance on through-deck welding parameters, including recommended parameter adjustment ranges for different deck thicknesses. This was not formally addressed in D1.1:2020 and was left to the Engineer of Record or contractor procedure.

Preheat Requirements

D1.1:2025 updates the minimum preheat temperature table for stud welding on ASTM A709 bridge steel grades. Some high-strength grades now require preheat at higher ambient temperatures than the previous edition specified.

What You Should Do

  • Review your existing WPS documents for compliance with D1.1:2025 if projects reference the new edition
  • Confirm with your EOR which edition of D1.1 governs your project
  • Update preheat procedures for A709 HPS grades if applicable
  • Ask us about updated WPS/PQR documentation for D1.1:2025-governed work